Sunking PCB

Materials Library

From standard FR4 to ceramic, PTFE, hydrocarbon/ceramic and polyimide — we work with a wide range of laminate suppliers.

At Sunking Circuits we offer many types of PCB materials, from standard FR4 to Ceramic Polymer, Ceramic/PTFE, Hydrocarbon/Ceramic, PTFE Composite and Polyimide. Your application should influence your material choice — for RF/microwave, signal integrity or temperature cycling. Contact us for suppliers and types not listed here.

IsolaRogersPanasonicVentecITEQTaconicNelcoArlonKingboard 建滔
TypeManufacturerProductTg (°C)Td (°C)DkDfApplication
FR4IsolaFR408HR1903603.680.0092Signal Integrity
FR4Isola370HR1803404.170.015–0.025Standard
FR4IsolaFR4081803603.670.012Signal Integrity
FR4IsolaItera MT402003603.450.0031Signal Integrity / RF
FR4IsolaAstra MT772003603.00.0017RF / Microwave
FR4IsolaTachyon 100G1803603.040.0021RF / Microwave
FR4ITEQIT180A1753454.40.015Standard
FR4VentecVT-421403104.30.015Standard
FR4VentecVT-471803554.270.016Standard
FR4VentecVT-4811553454.30.015Standard
FR4VentecVT-4471803804.350.013Standard (Halogen-Free)
FR4VentecVT-464(D)1604003.0–3.60.004–0.008Signal Integrity (Halogen-Free)
FR4Kingboard 建滔KB-6167F1753504.50.017Standard
FR4NelcoN4000-13 EP SI2103503.3–3.70.007–0.008Signal Integrity
FR4PanasonicMegtron 41763603.90.005Signal Integrity
FR4PanasonicMegtron 61854103.710.002Signal Integrity
FR4PanasonicMegtron 72004003.630.002Signal Integrity
PolyimideArlonArlon 85N2504074.20.01Temperature Cycling
PolyimideVentecVT-9012503904.050.013Temperature Cycling
PolyimideIsolaP95/P252604163.760.0179Temperature Cycling
PolyimideVentecVT-90H2503904.050.013Temperature Cycling
Ceramic PolymerRogersTMM10N/A4259.20.0022RF / Microwave
Ceramic PolymerRogersTMM10iN/A4259.80.002RF / Microwave
Ceramic PolymerRogersTMM13iN/A42512.850.0019RF / Microwave
Ceramic / PTFERogersRT/duroid 6002N/A5002.940.0012RF / Microwave
Ceramic / PTFERogersRO3003N/A5003.00.0013RF / Microwave
Ceramic / PTFERogersRO3006N/A5006.150.002RF / Microwave
Ceramic / PTFERogersRO3010N/A50010.20.0022RF / Microwave
Ceramic / PTFERogersRT/duroid 6006N/A5006.150.0027RF / Microwave
Ceramic / PTFERogersRT/duroid 6010N/A50010.20.0023RF / Microwave
Hydrocarbon / CeramicRogersRO4003C2803903.380.0027RF
Hydrocarbon / CeramicRogersRO4350B2804253.480.0037RF
Hydrocarbon / CeramicRogersRO4450F2803903.520.004RF
PTFE CompositeRogersRT/duroid 5870/5880N/A5002.330.0012RF / Microwave
PTFE CompositeTaconicTLY-5N/AN/A2.200.0009RF / Microwave

Values are typical; consult the manufacturer datasheet for complete and accurate data. This is not an all-inclusive list — contact us for other suppliers and types.