Sunking PCB

Products

Aluminum PCB

Aluminum Base Thickness
0.8mm-3.0mm
Thermal Conductivity
1.0-3.0 W/m·K
Copper Thickness
1oz-6oz
Aluminum PCB

Related board selection

For board selection, review the related page below and confirm against your project requirements.

Technical Specifications

Technical Specifications
SpecificationValue
Aluminum Base Thickness0.8mm-3.0mm
Thermal Conductivity1.0-3.0 W/m·K
Copper Thickness1oz-6oz
Surface FinishHASL/ENIG/OSP
Board SizeMax. 1500×600mm
Dielectric Withstand Voltage≥3000V

Product Features

  • Aluminum alloy base
  • Cost-effective thermal solution
  • LED lighting standard
  • 1-4 layers available
  • Thermal conductivity 1-3W/mK
  • V-cut scoring available

Applications

LED Luminaires
LED Displays
Power Adapters
Automotive Lighting
Traffic Signal Lights
Outdoor Lighting

FAQ

How are project parameters confirmed?
  • Project-specific manufacturability review against fabrication data and acceptance requirements.
Which surface finishes can be reviewed?
  • Finish, supply scope and acceptance criteria confirmed in project documents.

Need a quote for Aluminum PCB?

Upload your Gerber files and we'll quote within 1 hour for simple boards, 24 hours for complex builds.

Get Quote Now